BSI EN ISO Corrosion Related Standards |
||
|
Standard Number |
Standard Title |
|
| BS 7545:1991, ISO 8407:1991 | Method for removal of corrosion products from corrosion test specimens of metals and alloys | |
| BS EN ISO 4541:1995 | Metallic and other non-organic coatings. Corrodkote test (CORR test) | |
| BS EN 3026:1994 | Test method for dry film lubricants. Corrosion test on steel specimens | |
| BS EN 3212:1995 | Paints and varnishes. Corrosion test by alternate immersion in a buffered sodium chloride solution | |
| BS ISO 11907-2:1995 | Plastics. Smoke generation. Determination of the corrosivity of fire effluents. Static method | |
| BS EN 60654-4:1998, IEC 60654-4:1987 | Operating conditions for industrial-process measurement and control equipment. Corrosive and erosive influences | |
| BS ISO 11907-4:1998 | Plastics. Smoke generation. Determination of the corrosivity of fire effluents. Dynamic decomposition method using a conical radiant heater | |
| BS ISO 11907-3:1998 | Plastics. Smoke generation. Determination of the corrosivity of fire effluents. Dynamic decomposition method using a travelling furnace | |
| BS EN ISO 3651-1:1998 | Determination of resistance to intergranular corrosion of stainless steels. Austenitic and ferritic-austenitic (duplex) stainless steels. Corrosion test in nitric acid medium by measurement of loss in mass (Huey test) | |
| BS EN ISO 3651-2:1998 | Determination of resistance to intergranular corrosion of stainless steels. Ferritic, austenitic and ferritic-austenitic (duplex) stainless steels. Corrosion test in media containing sulfuric acid | |
| BS EN ISO 12944-4:1998 | Paints and varnishes. Corrosion protection of steel structures by protective paint systems. Types of surface and surface preparation | |
| BS EN ISO 12944-8:1998 | Paints and varnishes. Corrosion protection of steel structures by protective paint systems. Development of specifications for new work and maintenance | |
| BS EN ISO 12944-2:1998 | Paints and varnishes. Corrosion protection of steel structures by protective paint systems. Classification of environments | |
| BS EN 10283:1999 | Corrosion resistant steel castings | |
| BS EN ISO 9455-15:2000 | Soft soldering fluxes. Test methods. Copper corrosion test | |
| BS EN 61701:2000, IEC 61701:1995 | Salt mist corrosion testing of photovoltaic (PV) modules | |
| BS EN ISO 10289:2001 | Methods for corrosion testing of metallic and other inorganic coatings on metallic substrates. Rating of test specimens and manufactured articles subjected to corrosion tests | |
| BS EN 12508:2000 | Corrosion protection of metals and alloys. Surface treatment, metallic and other inorganic coatings. Vocabulary | |
| BS EN 13858:2003 | Corrosion protection of metals. Non-electrolytically applied zinc flake coatings on iron or steel components | |
| BS ISO 4524-2:2000 | Metallic coatings. Test methods for electrodeposited gold and gold alloy coatings. Mixed flowing gas (MFG) environmental tests | |
| BS EN 60512-11-6:2002 | Connectors for electronic equipment. Tests and measurements. Climatic tests. Test 11f. Corrosion, salt mist | |
| BS ISO/TS 12928:1999, ISO/TS 12928:1999 | Lubricants, industrial oils and related products (class L). Family R (products for temporary protection against corrosion). Guidelines for establishing specifications | |
| BS EN 4113:2001 | Aerospace series. Clamps, loop (P type) in corrosion resisting steel with rubber cushioning. Dimensions and masses | |
| BS EN 12502-5:2004 | Protection of metallic materials against corrosion. Guidance on the assessment of corrosion likelihood in water distribution and storage systems. Influencing factors for cast iron, unalloyed and low alloyed steels | |
| BS EN ISO 13402:2001, BS 7891:1997 | Surgical and dental hand instruments. Determination of resistance against autoclaving, corrosion and thermal exposure | |
| BS EN 1965-2:2001 | Structural adhesives. Corrosion. Determination and classification of corrosion to a brass substrate | |
| BS EN 1965-1:2001 | Structural adhesives. Corrosion. Determination and classification of corrosion to a copper substrate | |
| BS EN 60512-11-7:2003 | Connectors for electronic equipment. Tests and measurements. Flowing mixed gas corrosion test | |
| BS EN 12501-1:2003 | Protection of metallic materials against corrosion. Corrosion likelihood in soil. General | |
| BS EN 12502-1:2004 | Protection of metallic materials against corrosion. Guidance on the assessment of corrosion likelihood in water distribution and storage systems. General | |
| BS EN 12501-2:2003 | Protection of metallic materials against corrosion. Corrosion likelihood in soil. Low alloyed and non alloyed ferrous materials | |
| BS EN 12502-2:2004 | Protection of metallic materials against corrosion. Guidance on the assessment of corrosion likelihood in water distribution and storage systems. Influencing factors for copper and copper alloys | |
| BS EN 12502-3:2004 | Protection of metallic materials against corrosion. Guidance on the assessment of corrosion likelihood in water distribution and storage systems. Influencing factors for hot dip galvanised ferrous materials | |
| BS EN 12502-4:2004 | Protection of metallic materials against corrosion. Guidance on the assessment of corrosion likelihood in water distribution and storage systems. Influencing factors for stainless steels | |
| BS EN ISO 22775:2004 | Footwear. Test methods for accessories. Metallic accessories. Corrosion resistance | |
| BS EN 60695-5-1:2003 | Fire hazard testing. Assessment of potential corrosion damage by fire effluent. General guidance | |
| BS EN 10088-3:2005 | Stainless steels. Technical delivery conditions for semi-finished products, bars, rods, wire, sections and bright products of corrosion resisting steels for general purposes | |
| BS ISO 11844-2:2005 | Corrosion of metals and alloys. Classification of low corrosivity of indoor atmospheres. Determination of corrosion attack in indoor atmospheres | |
| BS ISO 11844-3:2006 | Corrosion of metals and alloys. Classification of low corrosivity of indoor atmospheres. Measurement of environmental parameters affecting indoor corrosivity | |
| BS ISO 4404-1:2001 | Petroleum and related products. Determination of the corrosion resistance of fire-resistant hydraulic fluids. Water-containing fluids | |
| BS EN ISO 7539-7:2005 | Corrosion of metals and alloys. Stress corrosion testing. Method for slow strain rate testing | |
| BS EN ISO 4404-2:2003 | Petroleum and related products. Determination of the corrosion resistance fire-resistant hydraulic fluids. Non-aqueous fluids | |
| BS EN ISO 10271:2001 | Dental metallic materials. Corrosion test methods | |
| BS EN ISO 4623-1:2002, BS 3900-F13:2002 | Paints and varnishes. Determination of resistance to filiform corrosion. Steel substrates | |
| BS ISO 11303:2002 | Corrosion of metals and alloys. Guidelines for selection of protection methods against atmospheric corrosion | |
| BS M 93:2005 | Protection of magnesium-rich alloys against corrosion. Specification | |
| BS ISO 7539-9:2003 | Corrosion of metals and alloys. Stress corrosion testing. Preparation and use of pre-cracked specimens for tests under rising load or rising displacement | |
| BS EN ISO 7539-6:2003 | Corrosion of metals and alloys. Stress corrosion testing. Preparation and use of pre-cracked specimens for tests under constant load or constant displacement | |
| BS ISO 16701:2003 | Corrosion of metals and alloys. Corrosion in artificial atmosphere. Accelerated corrosion test involving exposure under controlled conditions of humidity cycling and intermittent spraying of a salt solution | |
| BS EN 12472:2005 | Method for the simulation of wear and corrosion for the detection of nickel release from coated items | |
| BS EN 14832:2005 | Petroleum and related products. Determination of the oxidation stability and corrosivity of fire-resistant phosphate ester fluids | |
| BS EN ISO 4628-10:2003, BS 3900-H10:2003 | Paints and varnishes. Evaluation of degradation of coatings. Designation of quantity and size of defects, and of intensity of uniform changes in appearance. Assessment of degree of filiform corrosion | |
| BS EN 14868:2005 | Protection of metallic materials against corrosion. Guidance on the assessment of corrosion likelihood in closed water circulation systems | |
| BS ISO 16784-1:2006 | Corrosion of metals and alloys. Corrosion and fouling in industrial cooling water systems. Guidelines for conducting pilot-scale evaluation of corrosion and fouling control additives for open recirculating cooling water systems | |
| BS EN ISO 4623-2:2004, BS 3900-F20:2004 | Paints and varnishes. Determination of resistance to filiform corrosion. Aluminium substrates | |
| BS EN 14483-4:2004 | Vitreous and porcelain enamels. Determination of resistance to chemical corrosion. Determination of resistance to chemical corrosion by alkaline liquids using a cylindrical vessel | |
| BS EN 3841-402:2004 | Aerospace series. Circuit breakers. Test methods. Corrosion | |
| BS 2000-112:2005, IP 112:2005 | Methods of test for petroleum and its products. Determination of corrosiveness to copper of lubricating grease. Copper strip method | |
| BS EN 2435-001:2006 | Aerospace series. Paints and varnishes. Corrosion resistant chromated two component cold curing primer. Minimum requirements | |
| BS ISO 11844-1:2006 | Corrosion of metals and alloys. Classification of low corrosivity of indoor atmospheres. Determination and estimation of indoor corrosivity | |
| PD 6484:1979 | Commentary on corrosion at bimetallic contacts and its alleviation | |
| BS 3745:1970 | Method for the evaluation of results of accelerated corrosion tests on metallic coatings | |
| BS 6413-8:1988, ISO 6743-8:1987 | Lubricants, industrial oils and related products (class L). Classification for family R (temporary protection against corrosion) | |
| BS 5117-0:1992 | Testing corrosion inhibiting, engine coolant concentrate ('antifreeze'). General introduction | |
| BS EN ISO 7441:1995 | Corrosion of metals and alloys. Determination of bimetallic corrosion in outdoor exposure corrosion tests | |
| BS EN ISO 8565:1995 | Metals and alloys. Atmospheric corrosion testing. General requirements for field tests | |
| BS EN ISO 9400:1996 | Nickel-based alloys. Determination of resistance to intergranular corrosion | |
| BS 2000-315:1998, ISO 5662:1997 | Methods of test for petroleum and its products. Petroleum products. Electrical insulating oils. Detection of corrosive sulfur | |
| BS EN 12500:2000 | Protection of metallic materials against corrosion. Corrosion likelihood in atmospheric environment. Classification, determination and estimation of corrosivity of atmospheric environments | |
| BS 7195:1989 | Guide for prevention of corrosion of metals caused by vapours from organic materials | |
| BS EN ISO 7539-2:1995 | Corrosion of metals and alloys. Stress corrosion testing. Preparation and use of bent-beam specimens | |
| BS EN ISO 7539-3:1995, U | Corrosion of metals and alloys. Stress corrosion testing. Preparation and use of U-bend specimens | |
| BS EN ISO 7539-5:1995 | Corrosion of metals and alloys. Stress corrosion testing. Method for the preparation and use of C-ring specimens | |
| BS EN ISO 7539-4:1995 | Corrosion of metals and alloys. Stress corrosion testing. Preparation and use of uniaxially loaded tension specimens | |
| BS EN ISO 7384:1995 | Corrosion tests in artificial atmospheres. General requirements | |
| BS EN ISO 14713:1999 | Protection against corrosion of iron and steel in structures. Zinc and aluminium coatings. Guidelines | |
| BS EN ISO 7539-1:1995 | Corrosion of metals and alloys. Stress corrosion testing. General guidance on testing procedures | |
| BS 4553-3:1998 | Specification for 600/1000 V single-phase split concentric electric cables. Cables having thermosetting insulation and low emission of smoke and corrosive gases when affected by fire | |
| BS EN 12487:2000 | Corrosion protection of metals. rinsed and non-rinsed chromate conversion coatings on aluminium and aluminium alloys | |
| BS EN 60068-2-60:1996, IEC 60068-2-60:1995 | Environmental testing. Test methods. Test Ke. Flowing mixed gas corrosion test | |
| BS 5466-7:1982, ISO 4542-1981 | Methods for corrosion testing of metallic coatings. Guidance on stationary outdoor exposure corrosion tests | |
| BS EN ISO 2160:1998, BS 2000-154:1999, ISO 2160:1998 | Petroleum products. Corrosiveness to copper. Copper strip test | |
| BS ISO 11907-1:1998 | Plastics. Smoke generation. Determination of the corrosivity of fire effluents. Guidance | |
| BS EN 10088-2:2005 | Stainless steels. Technical delivery conditions for sheet/plate and strip of corrosion resisting steels for general purposes | |
| BS EN ISO 10156-2:2005 | Gas cylinders. Gases and gas mixtures. Determination of oxidizing ability of toxic and corrosive gases and gas mixtures | |
| BS EN ISO 6251:1998, BS 2000-411:1998, ISO 6251:1996 | Liquid petroleum gases. Corrosiveness to copper. Copper strip test | |
| BS ISO 15329:2006 | Corrosion of metals and alloys. Anodic test for evaluation of intergranular corrosion susceptibility of heat-treatable aluminium alloys | |
| BS 4601:1970 | Specification for electroplated coatings of nickel plus chromium on plastics materials | |
| BS 5117-2.1:1985 | Testing corrosion inhibiting, engine coolant concentrate ('antifreeze'). Methods of test for corrosion inhibition performance. General procedures | |
| BS 5117-2.5:1985 | Testing corrosion inhibiting, engine coolant concentrate ('antifreeze'). Methods of test for corrosion inhibition performance. Field test | |
| BS EN ISO 6509:1995 | Corrosion of metals and alloys. Determination of dezincification resistance of brass | |
| BS ISO 10270:1995 | Corrosion of metals and alloys. Aqueous corrosion testing of zirconium alloys for use in nuclear power reactors | |
| BS ISO 11463:1995 | Corrosion of metals and alloys. Evaluation of pitting corrosion | |
| BS ISO 11846:1995 | Corrosion of metals and alloys. Determination of resistance to intergranular corrosion of solution heat-treatable aluminium alloys | |
| BS EN 1618:1997 | Catheters other than intravascular catheters. Test methods for common properties | |
| BS ISO 11782-1:1998 | Corrosion of metal and alloys. Corrosion fatigue testing. Cycles to failure testing | |
| BS ISO 11782-2:1998 | Corrosion of metal and alloys. Corrosion fatigue testing. Crack propagation testing using precracked specimens | |
| BS EN ISO 11130:1999 | Corrosion of metals and alloys. Alternate immersion test in salt solution | |
| BS ISO 7539-8:2000 | Corrosion of metals and alloys. Stress corrosion testing. Preparation and use of specimens to evaluate weldments | |
| BS 6338:1982, ISO 4520-1981 | Specification for chromate conversion coatings on electroplated zinc and cadmium coatings | |
| BS EN ISO 8044:2000 | Corrosion of metals and alloys. Basic terms and definitions | |
| BS ISO 15324:2000 | Corrosion of metals and alloys. Evaluation of stress corrosion cracking by the drop evaporation test | |
| BS 7211:1998 | Electric cables. Thermosetting insulated, non-armoured cables for voltages up to and including 450/750 V, for electric power, lighting and internal wiring, and having low emission of smoke and corrosive gases when affected by fire | |
| BS 6724:1997 | Electric cables. Thermosetting insulated, armoured cables for voltages of 600/1000 V and 1900/3300 V, having low emission of smoke and corrosive gases when affected by fire | |
| BS AU 180-6:1982, ISO 6315-1980 | Brake linings. Method for assessment of seizure to ferrous mating surface due to corrosion | |
| BS EN ISO 4536:1995 | Metallic and non-organic coatings on metallic substrates. Saline droplets corrosion test (SD test) | |
| BS ISO 4404:1998 | Petroleum and related products. Determination of the corrosion resistance of water-containing fire-resistant fluids for hydraulic systems | |
| BS EN 12329:2000 | Corrosion protection of metals. Electrodeposited coatings of zinc with supplementary treatment on iron or steel | |
| BS EN 990:2002 | Test methods for verification of corrosion protection of reinforcement in autoclaved aerated concrete and lightweight aggregate concrete with open structure | |
| BS ISO 17864:2005 | Corrosion of metals and alloys. Determination of the critical pitting temperature under potentiostatic control | |
| BS ISO 15710:2002 | Paints and varnishes. Corrosion testing by alternate immersion in and removal from a buffered sodium chloride solution | |
| BS EN 14483-3:2004 | Vitreous and porcelain enamels. Determination of resistance to chemical corrosion. Determination of resistance to chemical corrosion by alkaline liquids using a hexagonal vessel | |
| BS EN 14483-5:2004 | Vitreous and porcelain enamels. Determination of resistance to chemical corrosion. Determination of resistance to chemical corrosion in closed systems | |
| BS EN 12373-19:2001 | Aluminium and aluminium alloys. Anodizing. Rating system for the evaluation of pitting corrosion. Grid method | |
| BS EN 12373-18:2001 | Aluminium and aluminium alloys. Anodizing. Rating system for the evaluation of pitting corrosion. Chart method | |
| BS EN 2436-006:2006 | Aerospace series. Paints and varnishes. Corrosion resistant chromate-free two component cold curing epoxy primer. High corrosion resistance for military application | |
| BS EN 50162:2004 | Protection against corrosion by stray current from direct current systems | |
| BS EN ISO 17834:2003 | Thermal spraying. Coatings for protection against corrosion and oxidation at elevated temperatures | |
| BS 8436:2004 | Electric cables. 300/500 V screened electric cables having low emission of smoke and corrosive gases when affected by fire, for use in walls, partitions and building voids. Multicore cables | |
| BS ISO 16151:2005 | Corrosion of metals and alloys. Accelerated cyclic tests with exposureto acidified salt spray, "dry" and "wet" conditions | |
| BS EN 2435-002:2006 | Aerospace series. Paints and varnishes. Corrosion resistant chromated two component cold curing primer. High corrosion resistance | |
| BS EN 2435-003:2006 | Aerospace series. Paints and varnishes. Corrosion resistant chromated two component cold curing primer. High corrosion and fluid resistance | |
| BS EN 2435-004:2006 | Aerospace series. Paints and varnishes. Corrosion resistant chromated two component cold curing primer. High corrosion and fluid resistance with surface preparation tolerance | |
| BS EN 2436-002:2006 | Aerospace series. Paints and varnishes. Corrosion resistant chromate-free two component cold curing primer. High corrosion resistance | |
| BS 5117-2.2:1985 | Testing corrosion inhibiting, engine coolant concentrate ('antifreeze'). Methods of test for corrosion inhibition performance. Glassware tests | |
| BS 3130-1:1989 | Glossary of packaging terms. General (including auxiliary materials) | |
| BS EN ISO 4538:1995 | Metallic coatings. Thioacetamide corrosion test (TAA test) | |
| BS 5735:1979, IEC 60426:1973 | Test methods for determining electrolytic corrosion with electrical insulating materials | |
| BS EN 2335:1990 | Specification for bearings-spherical plain in corrosion resisting steel without assembly slot. Dimensions and loads | |
| BS 5117-2.4:1985 | Testing corrosion inhibiting, engine coolant concentrate ('antifreeze'). Methods of test for corrosion inhibition performance. Static engine test | |
| BS EN ISO 9227:2006 | Corrosion tests in artificial atmospheres. Salt spray tests | |
| BS EN 2436-003:2006 | Aerospace series. Paints and varnishes. Corrosion resistant chromate-free two component cold curing primer. High corrosion and fluid resistance | |
| BS EN 2436-004:2006 | Aerospace series. Paints and varnishes. Corrosion resistant chromate-free two component cold curing primer. High corrosion and fluid resistance with surface preparation tolerance | |
| BS ISO 17475:2005 | Corrosion of metals and alloys. Electrochemical test methods. Guidelines for conducting potentiostatic and potentiodynamic polarization measurements | |
| BS 7835:2000 | Specification for armoured cables with extruded cross-linked polyethylene or ethylene propylene rubber insulation for rated voltages from 3.8/6.6 kV up to 19/33 kV having low emission of smoke and corrosive gases when affected by fire | |
| BS 5117-2.6:1992 | Testing corrosion inhibiting, engine coolant concentrate ('antifreeze'). Methods of test for corrosion inhibition performance. Test for corrosion of cast aluminium alloys under heat-transfer conditions | |
| BS 6580:1992 | Specification for corrosion inhibiting, engine coolant concentrate ('antifreeze') | |
| BS EN 2435-005:2006 | Aerospace series. Paints and varnishes. Corrosion resistant chromated two component cold curing primer. High corrosion resistance for military application | |
| BS EN 12330:2000 | Corrosion protection of metals. Electrodeposited coatings of cadmium on iron or steel | |
| BS ISO 5952:2005 | Continuously hot-rolled steel sheet of structural quality with improved atmospheric corrosion resistance | |
| BS EN ISO 9455-12:1994 | Soft soldering fluxes. Test methods. Steel tube corrosion test | |
| BS EN ISO 11306:1998 | Corrosion of metals and alloys. Guidelines for exposing and evaluating metals and alloys in surface sea water | |
| BS EN 3665:1997 | Test methods for paints and varnishes. Filiform corrosion resistance test on aluminium alloys | |
| BS EN 14483-1:2004 | Vitreous and porcelain enamels. Determination of resistance to chemical corrosion. Determination of resistance to chemical corrosion by acids at room temperature | |
| DD CEN/TS 15280:2006 | Evaluation of a.c. corrosion likelihood of buried pipelines. Application to cathodically protected pipelines | |
| BS EN 2436-001:2006 | Aerospace series. Paints and varnishes. Corrosion resistant chromate-free two component cold curing primer. Basic requirements | |
| BS 3924:1978 | Specification for pressure-sensitive adhesive tapes for electrical insulating purposes | |
| BS 4147:1980 | Specification for bitumen-based hot-applied coating materials for protecting iron and steel, including suitable primers where required | |
| BS EN ISO 12944-6:1998 | Paints and varnishes. Corrosion protection of steel structures by protective paint systems. Laboratory performance test methods | |
| BS EN 1670:1998 | Building hardware. Corrosion resistance. Requirements and test methods | |
| BS EN ISO 4543:1995 | Metallic and other non-organic coatings. General rules for corrosion tests applicable for storage conditions | |
| BS EN 2516:1997 | Passivation of corrosion resisting steels and decontamination of nickel base alloys | |
| BS EN 61076-3-101:1998, IEC 61076-3-101:1997 | Connectors with assessed quality, for use in d.c., low-frequency analogue and in digital high speed data applications. Rectangular connectors. Detail specification for a range of shielded connectors with trapezoidal shaped shells and non-removable rectangular contacts on a 1,27 x 2,54 mm centre-line | |
| BS EN ISO 12944-1:1998 | Paints and varnishes. Corrosion protection of steel structures by protective paint systems. General introduction | |
| BS EN 1403:1998 | Corrosion protection of metals. Electrodeposited coatings. Method of specifying general requirements | |
| BS EN 60793-1-33:2002, IEC 60793-1-33:2001 | Optical fibres. Measurement methods and test procedures. Stress corrosion susceptibility. Section 33 Stress corrossion susceptibility | |
| BS 3900-F19:2000, ISO 11997-2:2000 | Methods of test for paint. Durability tests on paint films. Determination of resistance to cyclic corrosion conditions. Wet (salt fog)/dry/humidity/UV light. Part F19: Determination of resistance to cyclic corrosion conditions - Wet (salt fog)/dry/humidity/UV light | |
| BS 2011-2.2Kd:1984, IEC 60068-2-46:1982 | Environmental testing. Guidance. Test Kd. Guidance on Test Kd: Hydrogen sulphide test for contacts and connections | |
| DD ENV 12837:2000 | Paints and varnishes. Qualification of inspectors for corrosion protection of steel structures by protective paint systems | |
| DD ENV ISO 8502-1:2001 | Preparation of steel substrates before application of paints and related products. Tests for the assessment of surface cleanliness. Field test for soluble iron corrosion products | |
| BS EN 60512-11-14:2003 | Connectors for electronic equipment. Tests and measurements. Climatic tests. Flowing single gas corrosion test | |
| BS EN 14483-2:2004 | Vitreous and porcelain enamels. Determination of resistance to chemical corrosion. Determination of resistance to chemical corrosion by boiling acids, neutral liquids and/or their vapours | |
| BS EN 4590:2005 | Aerospace series. Retainers, spring, sheet metal, for self-locking barrel nuts, in corrosion resisting steel, passivated | |
| BS EN ISO 10062:1995 | Corrosion test in artificial atmospheres at very low concentrations of polluting gas(es) | |
| BS ISO 11997-1:2005, BS 3900-F18:2005 | Paints and varnishes. Determination of resistance to cyclic corrosion conditions. Wet (salt fog)/dry/humidity | |
| BS EN 2436-005:2006 | Aerospace series. Paints and varnishes. Corrosion resistant chromate-free two component cold curing primer. For exterior use with surface preparation tolerance | |
| DD ENV 12923-1:1998 | Advanced technical ceramics. Monolithic ceramics. General practice for undertaking corrosion tests | |
| BS 5493:1977 | Code of practice for protective coating of iron and steel structures against corrosion | |
| BS 2569-2:1965 | Specification for sprayed metal coatings. Protection of iron and steel against corrosion and oxidation at elevated temperatures | |
| BS 5117-1.1:1985 | Testing corrosion inhibiting, engine coolant concentrate ('antifreeze'). Methods of test for determination of physical and chemical properties. Ancillary procedures | |
| BS 5117-1.2:1985 | Testing corrosion inhibiting, engine coolant concentrate ('antifreeze'). Methods of test for determination of physical and chemical properties. Determination of boiling point | |
| BS 5117-1.3:1985 | Testing corrosion inhibiting, engine coolant concentrate ('antifreeze'). Methods of test for determination of physical and chemical properties. Determination of freezing point | |
| BS 5117-1.4:1985 | Testing corrosion inhibiting, engine coolant concentrate ('antifreeze'). Methods of test for determination of physical and chemical properties. Determination of foaming characteristics | |
| BS M 58:1986, ISO 8080-1985 | Specification for anodic coating of titanium and titanium alloys by the sulphuric acid process | |
| BS 1683:1987 | Specification for coated aluminium foil for wrapping processed cheese | |
| BS AU 194:1984 | Specification for performance of electrical connections between towing vehicles and trailers | |
| BS EN 12540:2000 | Corrosion protection of metals. Electrodeposited coatings of nickel, nickel plus chromium, copper plus nickel and copper plus nickel plus chromium | |
| BS EN 846-13:2001 | Methods of test for ancillary components for masonry. Determination of resistance to impact, abrasion and corrosion of organic coatings | |
| BS EN ISO 4628-8:2005, BS 3900-H8:2005 | Paints and varnishes. Evaluation of degradation of coatings. Designation of quantity and size of defects, and of intensity of uniform changes in appearance. Assessment of degree of delamination and corrosion around a scribe | |
| BS EN ISO 12944-5:1998 | Paints and varnishes. Corrosion protection of steel structures by protective paint systems. Protective paint systems | |
| BS EN ISO 12944-3:1998 | Paints and varnishes. Corrosion protection of steel structures by protective paint systems. Design considerations | |
| BS ISO 16428:2005 | Implants for surgery. Test solutions and environmental conditions for static and dynamic corrosion tests on implantable materials and medical devices | |
| BS 873-1:1983 | Road traffic signs and internally illuminated bollards. Methods of test | |
| BS EN ISO 12944-7:1998 | Paints and varnishes. Corrosion protection of steel structures by protective paint systems. Execution and supervision of paintwork | |
| BS EN 14879-1:2005 | 0rganic coating systems and linings for protection of industrial apparatus and plants against corrosion caused by aggressive media. Terminology, design and preparation of substrate | |
| BS 5117-1.5:1992 | Testing corrosion inhibiting, engine coolant concentrate ('antifreeze'). Methods of test for determination of physical and chemical properties. Coolant hard water stability test | |
| BS EN 10025-5:2004 | Hot rolled products of structual steels. Technical delivery conditons for structural steels with improved atmospheric corrosion resistance | |
| BS 7870-2:1999 | LV and MV polymeric insulated cables for use by distribution and generation utilities. Methods of test | |
| BS 7655-6.1:1997 | Specification for insulating and sheathing materials for cables. Thermoplastic sheathing compounds having low emission of corrosive gases, and suitable for use in cables having low emission of smoke when affected by fire. General application thermoplastic types | |
| BS 3146-2:1975 | Specification for investment castings in metal. Corrosion and heat resisting steels, nickel and cobalt base alloys | |
| BS EN 12068:1999 | Cathodic protection. External organic coatings for the corrosion protection of buried or immersed steel pipelines used in conjunction with cathodic protection. Tapes and shrinkable materials | |
| 93/201088 DC | prEN 50114. Materials and size requirements for earth electrodes from the corrosion point of view | |
| 93/704327 DC | Aerospace series. Aluminium alloy AL-P2024-T351. Sheet and strip. 0,8 mm≤a≤6 mm (prEN 3999) | |
| 93/706720 DC | Aerospace series. Vacuum deposition of cadmium (prEN 2535) | |
| 93/706752 DC | Aerospace series. Aluminium alloy AL-P7475-T7351, plate, 6 mm | |
| 93/714443 DC | Aerospace series. Aluminium alloy AL-P7075-T73. Die forgings a ≤ 125 mm (prEN 3880) | |
| 93/714444 DC | Aerospace series. Aluminium alloy AL-P7075-T73. Hand forgings a ≤ 125 mm (prEN 3881) | |
| 93/717455 DC | Aerospace series. Screws, pan head, slotted, threaded to head, in corrosion resisting steel, passivated. Classification: 490 MPa (at ambient temperature)/425°C (prEN 4076) | |
| 93/717456 DC | Aerospace series. Screws, normal hexagon head, threaded to head, in heat and corrosion resisting steel, passivated. Classification: 900 MPa (at ambient temperature)/650°C (prEN 4077) | |
| 95/702085 DC | Petroleum and natural gas industries. Bolted bonnet steel gate valves for refinery and related applications. Basic requirements (ISO/DIS 10434) | |
| 95/715398 DC | Aerospace series. Metallic materials. Rules for drafting and presentation of test method standards. Part 7. Specific requirements for corrosion and stress-corrosion test method standard. (prEN 4261-7) | |
| 96/205308 DC | prEN 50245. Plugs and socket-outlets 16A 250V a.c. for household and similar purposes general requirements and dimensions variant 1 (3P + 2P) | |
| 96/205310 DC | prEN 50246. Plugs and socket-outlets 16A 250 V a.c. for household and similar purposes. Conversion adapters | |
| 96/709571 DC | Steel tubes and fittings for on and offshore pipelines. External three layer extruded polypropylene based coatings (prEN 10286) | |
| 96/709572 DC | Steel tubes and fittings for on and offshore pipelines. External fused polyethylene based coatings (prEN 10287) | |
| 96/713159 DC | Corrosion of metals and alloys. Guidelines for applying statistics to analysis corrosion data (ISO/DIS 14802) | |
| 97/700600 DC | Aerospace series. Electroless nickel plating of corrosion resistance steel (prEN 3839) | |
| 97/703738 DC | Aerospace series. Paints and varnishes. Corrosion resistant chromate-free two component cold curing primer. Part 3. High corrosion and fluid resistance (prEN 4405-003) | |
| 97/703737 DC | Aerospace series. Paints and varnishes. Corrosion resistant chromate-free two component cold curing primer. Part 2. High corrosion resistance (prEN 4405-002) | |
| 97/703739 DC | Aerospace series. Paints and varnishes. Corrosion resistant chromate-free two component cold curing primer. Part 4. High corrosion and fluid resistance with surface tolerance (prEN 4405-004) | |
| 97/703736 DC | Aerospace series. Paints and varnishes. Corrosion resistant chromate. Free two component cold curing primer. Part 1. Minimum requirements (prEN 4405-001) | |
| 97/104479 DC | prEN 12897. Water supply. Specification for indirectly heated unvented (closed) hot water storage systems | |
| 97/208495 DC | IEC 61640. HV gas-insulated transmission lines for rated voltages of 72,5 kV and above (IEC Document 17C/200/CDV) | |
| 97/717144 DC | ISO/DIS 9216. Aerospace. Nuts, hexagonal, slotted (castellated), for pulleys, in cadmium plated steel and corrosion resisting steel | |
| 97/717145 DC | ISO/DIS 9217. Aerospace. Washers, chamfered, with counterbore, for pulleys, in alloy steel and corrosion resisting steel. Dimensions and masses | |
| 97/717146 DC | ISO/DIS 9218. Aerospace. Washers, flat, for pulleys, in alloy steel and corrosion resisting steel. Dimensions and masses | |
| 97/719219 DC | Aerospace series. Aluminium alloy AL-P2014A-T3. Drawn tube for structural applications. 0,6 mm ≤ a ≤ 12,5 mm (prEN 3346) | |
| 97/719245 DC | Aerospace series. Aluminium alloy AL-P7050-T74. Die forgings. a ≤ 150 mm (prEN 2688) | |
| 97/719244 DC | Aerospace series. Aluminium alloy AL-P7010-T7451. Hand forgings. a ≤ 150 mm (prEN 2686) | |
| 97/719243 DC | Aerospace series. Aluminium alloy AL-P7010-T7651. Hand forgings. a ≤ 150 mm (prEN 2683) | |
| 97/719242 DC | Aerospace series. Alluminium alloy AL-P7010-T7452. Hand and die forgings. a ≤ 150 mm (prEN 2682) | |
| 97/719238 DC | Aerospace series. Aluminium alloy AL-P7075-T7352. Hand forgings. a ≤ 150 mm (prEN 2386) | |
| 97/719257 DC | Aerospace series. Aluminium AL-P7175-T7354. Die forgings. a ≤ 150 mm (prEN 4294) | |
| 97/719256 DC | Aerospace series. Aluminium AL-P7175-T73511. Extruded bar and section. a or D ≤ 150 mm (prEN 4293) | |
| 97/719252 DC | Aerospace series. Aluminium alloy AL-P2219-T851. Forgings. a ≤ 400 mm (prEN 4285) | |
| 97/719248 DC | Aerospace series. Aluminium AL-P7175-T7352. Hand and die forgings. a ≤ 150 mm (prEN 4278) | |
| 97/719247 DC | Aerospace series. Aluminium AL-P7175-T73. Hand and die forgings. a ≤ 125 mm (prEN 4277) | |
| 97/719246 DC | Aerospace series. Aluminium AL-P7175-T7351. Hand forgings. a ≤ 150 mm (prEN 4276) | |
| 97/109272 DC | prEN 13063. Chimneys. System chimneys with clay/ceramic flue liners or blocks | |
| 98/700452 DC | Aerospace series. Aluminium alloy AL-P7050-T7452. Die forgings a ≤ 150 mm (prEN 4448) | |
| 98/705334 DC | Method for electrochemical potentiokinetic reactivation test (based on Cihal's method) (ISO/CD 12732) | |
| 98/201910 DC | prEN 50297. Photoelectric control units for road and street lighting | |
| 98/103952 DC | BS EN 12209-3. Building hardware. Locks and latches. Part 3. Electromechanically operated locks and striking plates. Requirements and test methods (prEN 12209-3:1998) | |
| 98/710176 DC | Aerospace series. Paints and varnishes. Corrosion preventive two component cold curing coating for integral fuel tanks with medium fuel temperature (prEN 4451) | |
| 98/710177 DC | Aerospace series. Paints and varnishes. Corrosion preventive two component cold curing coating for integral tanks with high fuel temperature (prEN 4452) | |
| 98/712176 DC | Aerospace series. Aluminium alloy SL-P7475-T7351. Plate 6 mm ≤ a ≤ 100 mm (prEN 4457) | |
| 98/712171 DC | Aerospace series. Aluminium alloy AL-P7010-T76. Die forgings. a ≤ 200 mm (prEN 3339) | |
| 98/712165 DC | Aerospace series. Aluminium alloy AL-P7050-T7452 Hand forgings A ≤ 200 mm. (prEN 2690) | |
| 98/711596 DC | Steel tubes and fittings for onshore and offshore pipelines. External coatings by bitumen or coal tar derived materials (prEN 10300) | |
| 98/713242 DC | Aerospace series. Aluminium and aluminium alloy wrought products. Technical specification. Part 1. Plate (prEN 4400-1) | |
| 98/713306 DC | Aerospace series. Bolts, normal hexagonal head, close tolerance normal shank, short thread, in heat and corrosion resisting steel, passivated. Classification:1100 MPa (at ambient temperature)/425°C (prEN 3052) | |
| 98/716951 DC | Aerospace series. Studs, in titanium alloy TI-P64001, MoS2 coated, with serrated locking ring in corrosion resisting steel. Strength class. 1100 MPa (at ambient temperature) (prEN 4421) | |
| 00/711012 DC | prEN 2284. Aerospace series. Sulfuric acid anodising of Aluminium and wrought aluminium alloys | |
| 00/711011 DC | prEN 2101. Aerospace series. Chromic acid anodising of aluminium and wrought aluminium alloys | |
| 05/19974131 DC | BS EN 480-14. Admixtures for concrete, mortar and grout. Test methods. Part 14. Measurement of corrosion susceptibility of reinforcing steel in concrete. Potentiostatic electrochemical test method | |
| 01/208798 DC | IEC 60695-5-3 TS. Fire hazard testing. Part 5-3. Corrosion damage effects of fire effluent. Leakage current and metal loss test method | |
| 99/716256 DC | prEN 4405-06. Aerospace series. Paints and varnishes. Corrosion resistant chromate free two component cold during primer. Part 6. High corrosion resistance for military application | |
| 99/714426 DC | prEN 3106. Aerospace series. Sealants. Test methods. Determination of loss of mass and flexibility after fluid immersion | |
| 99/710287 DC | prEN 3105. Aerospace series. Sealants. Test methods. Determination of the corrosive effect of sealants on metallic materials | |
| 99/705627 DC | EN 10309. Steel tubes and fittings for onshore and offshore pipelines. External epoxy powder coating | |
| 91/81094 DC | Aerospace series. Molybdenum disulphide dry lubricants to be applied as a film. Technical specification (prEN 3021) | |
| 88/72193 DC | Aerospace series. Aluminium alloy sheet, strip, drawn and extruded sections and tubes (prENs 2092, 2124, 2126, 2128, 2317, 2319, 2320, 2393, 2419, 2640, 2655, 2703, 2704 and 2705) | |
| 04/19993251 DC | Aluminium and aluminium alloys. Castings. Chemical composition and mechanical properties | |
| 90/72764 DC | Aerospace series. Vulcanised rubbers. Tests on the susceptibility to corrosion of metals in contact with vulcanised rubbers in a damp atmosphere (prEN 2899) | |
| 99/710367 DC | IEC 4/156/CD. Hydraulic machines. Cavitation pitting evaluation in hydraulic turbines, storage pump and pump-turbines | |
| 99/710299 DC | prEN 4483. Aerospace. Sealing compounds, two-component polysulphide polymer base suitable for brush application for temperatures from -55°C to 95°C corrosion inhibiting. Properties | |
| 99/710300 DC | prEN 4484. Aerospace. Sealing compounds, two-component polysulphide polymer base suitable for blow gun or spatula application for temperatures from -55°C to 95°C corrosion inhibiting. Properties | |
| 99/710301 DC | prEN 4485. Aerospace. Sealing compounds, two-component polysulphide polymer base suitable for blow gun spatula or roll application for temperatures from -55°C to 95°C corrosion inhibiting. Properties | |
| 00/704670 DC | ECSS-Q-70-37. Space product assurance. Determination of the susceptibility of metals to stress. Corrosion cracking | |
| 00/714923 DC | prEN 10025-5. Hot rolled products of structural steels. Part 5. Technical delivery conditions for structural steels with improved atmospheric corrosion resistance | |
| 00/244337 DC | Electrochemical re-alkalisation and chloride extraction treatments for reinforced concrete. Part 1. Re-alkalisation CENELEC Document prEN 14038-1 | |
| 06/30036109 DC | BS 8442. Miscellaneous road traffic signs and devices. Requirements and test methods | |
| 00/124820 DC | Paints and varnishes. Corrosion protection of steel structures by protective paint systems. Measurement and acceptance criteria for the dry film thickness | |
| 01/122232 DC | BS ISO 20340. Paints and varnishes. Corrosion protection of steel structures by protective paint systems. Performance requirements for protective paint systems for off-shore and related structures | |
| 04/30057302 DC | BS EN ISO 9333. Dental brazing materials | |
| 05/30076043 DC | IEC 60454-2. Pressure sensitive adhesive tapes for e lectrical purposes. Part 2. Methods of test | |
| 04/30078970 DC | ISO 22088-1. Plastics. Determination of resistance to environmental stress cracking (ESC). Part 1. General guidance | |
| 04/30078973 DC | ISO 22088-2. Plastics. Determination of resistance to environmental stress cracking (ESC). Part 2. Constant tensile stress method | |
| 02/206714 DC | IEC 60695-5-3. Ed.1. Fire hazard testing. Part 5-3: Corrosion damage effects of fire effluent. Leakage current and metal loss test method | |
| 02/209094 DC | IEC 60335-2-XXX. Household and similar electrical appliances. Safety. Part 2-XXX: Particular requirements for commercial microwave appliances with insertion or contacting applicators | |
| 02/713774 DC | EN 10336. Continuously hot-dip coated and electrolytically coated strip and sheet of multiphase steels for cold forming. Technical delivery conditions | |
| 03/301401 DC | EN 14611. Space product assurance. Determination of the susceptibility of silver plated copper wire and cable to “red-plague” corrosion | |
| 06/30089837 DC | ISO 7866. Gas cylinders. Refillable seamless aluminium alloy gas cylinders. Design, construction and testing | |
| 03/302291 DC | EN 14629. Products and systems for the protection and repair of concrete structures. Test Methods. Determination of Chloride content in hardened concrete | |
| 03/314809 DC | EN ISO 13680. Petroleum and natural gas industries. Corrosion-resistant alloy seamless tubes for use as casing, tubing and coupling stock. Technical delivery conditions | |
| 03/305240 DC | BS ISO 16429. Implants for surgery. Long-term measurements of open-circuit potential to assess corrosion behaviour of metallic implantable materials and medical devices | |
| 06/30094368 DC | BS 4592-5. Industrial type flooring and stair treads. Part 5. Solidplate s in metal and glass reinforced plastics (GRP). Specification | |
| 06/30099306 DC | BS ISO 5832-9. Implants for surgery. Metallic materials. Part 9. Wrought high nitrogen stainless steel | |
| 05/30101483 DC | ISO 11486. Motorcycles. Methods for setting running resistance on a chassis dynamometer | |
| 03/317246 DC | ISO 2081. Metallic coatings. Electroplated coatings of zinc with supplementary treatments on iron or steel | |
| 06/30103169 DC | EN 12094-7. Fixed firefighting systems. Components for gas extinguishing systems. Part 7. Requirements and test methods for nozzles | |
| 06/30106554 DC | ISO 17872. Paints and varnishes. Guidelines for the introduction of scribe marks through coatings on metallic panels for corrosion | |
| 04/300071 DC | IEC 61300-2-26-A1 ED 1.0. Basic test and measurement procedures. Part 2-26. Tests. Salt mist | |
| 04/30107372 DC | BS EN 12183. Manual wheelchairs. Requirements and test methods | |
| 04/30107378 DC | EN 12184. Electrically powered wheelchairs, scooters and their chargers. Requirements and test methods | |
| 04/30109201 DC | EN 14879-2. Organic coating systems and linings for protection of industrial apparatus and plants against corrosion caused by aggressive media. Part 2. Coatings on metallic components | |
| 04/30109383 DC | ISO 8535-1. Compression-ignition engines. Steel tubes for high-pressure fuel injection pipes. Part 1. Requirements for seamless cold-drawn single-wall tubes | |
| 04/30110594 DC | ISO 12732. Corrosion of metals and alloys. Method for electrochemical potentiokinetic reactivation measurement using the double loop method (based on Cihal's method) | |
| 06/30110658 DC | EN ISO 3630-1. Dentistry. Root canal instruments. Part 1. General requirements and test methods | |
| 04/30112507 DC | ISO 7169. Aerospace. Separable tube fittings for fluid systems, for 24 cones, for pressures up to 3000 psi or 21 kPa. Procurement specification inch/metric | |
| 06/30112897 DC | EN 1670. Building hardware. Corrosion resistance. Requirements and test methods | |
| 04/30114371 DC | EN 10339. Steel tubes for onshore and offshore water pipelines. Internal liquid applied epoxy linings for corrosion protection | |
| 04/30116142 DC | ISO 4952. Structural steels with improved atmospheric corrosion resistance | |
| 04/30123574 DC | EN 14879-3. Organic coating systems and linings for protection of industrial apparatus and plants against corrosion caused by aggressive media. Part 3. Coatings on concrete components | |
| 04/30124042 DC | IEC 61300-2-26. Basic test and measurement procedures. Part 2-26. Tests. Salt mist | |
| 04/30124417 DC | EN 15081. Industrial valves. Mounting kits for part-turn valve actuator attachment | |
| 04/30125076 DC | EN 10111. Continuously hot rolled low carbon steel sheet and strip for cold forming. Technical delivery conditions | |
| 04/30125747 DC | IEC 60439-5 Ed.2. Low-voltage switchgear and controlgear assemblies. Part 5. Particular requirements for assemblies for power distribution in public networks | |
| 04/30125773 DC | EN 12923-1. Advanced technical ceramics. Monolithic ceramics. Part 1. General practice for undertaking corrosion tests | |
| 04/30125823 DC | ISO 17092. Fine ceramics (advanced ceramics, advanced technical ceramics). Determination of corrosion resistance of monolithic ceramics in acid and alkaline solutions | |
| 05/30126202 DC | EN 10088-4. Stainless steels. Part 4. Technical delivery conditions for sheet/plate and strip of corrosion resisting steels for construction purposes | |
| 05/30126205 DC | EN 10088-5. Stainless steels. Part 5. Technical delivery conditions for bars, rods, wire, sections and bright products of corrosion resisting steels | |
| 04/30126837 DC | BS ISO 6336-1. Calculation of load capacity of spur and helical gears. Part 1. Basic principles, introduction and general influence factors | |
| 05/30127517 DC | IEC 60454-3-11 ED 2. Pressure-sentive adhesive tapes for electrical purposes. Part 3. Specifications for individual materials | |
| 05/30129388 DC | ISO 21610. Corrosion of metals and alloys. Accelerated corrosion test for intergranular corrosion susceptibility of austenitic stainless steels | |
| 05/30131064 DC | EN 15189:2005. Ductile iron pipes, fittings and accessories. External polyurethane coating for pipes. Requirements and test methods | |
| 05/30131376 DC | BS EN 15183. Products and systems for the protection and repair of concrete structures. Test methods. Corrosion protection test | |
| 05/30131382 DC | BS EN 15184. Products and systems for the protection and repair of concrete structures. Test methods. Shear adhesion coated steel to concrete (pull-out test) | |
| 05/30131477 DC | ISO 17752. Corrosion of metals and alloys. Procedure to determine runoff rates of metals from materials as a result of atmospheric corrosion | |
| 05/30131749 DC | EN 15205. Determination of hexavalent chromium in corrosion protection layers. Qualitative analysis | |
| 05/30134748 DC | ISO 14521. Gears. Calculation of load capacity of wormgears | |
| 05/30135048 DC | EN 15257. Cathodic protection. Competence levels and certification of cathodic protection personnel | |
| 05/30135633 DC | IEC 60269-1 ED 4. Low-voltage fuses. Part 1. General requirements | |
| 05/30135642 DC | IEC 60269-2 ED 3. Low-voltage fuses. Part 2. Supplementary requirements for fuses for use by authorised persons (fuses mainly for industrial application). Examples of standardized systems of fuses A to I | |
| 05/30135649 DC | IEC 60269-4 ED 4. Low-voltage fuses. Part 4. Supplementary requirements for fuse-links for the protection of semiconductor devices | |
| 05/30136157 DC | IEC 60426 ED 2. Test methods for determining electrolytic corrosion with insuating materials | |
| 05/30138201 DC | ISO 12696. Cathodic protection of steel in concrete | |
| 05/30138231 DC | ISO 8407. Corrosion of metals and alloys. Removal of corrosion products from corrosion test specimens | |
| 05/30138471 DC | EN ISO 16276-2. Corrosion protection of steel structures by protective paint systems. Assessment of, and acceptance criteria for, the adhesion/cohesion (fracture strength) of a dry film. Part 2. Cross-cut testing and X-cut testing | |
| 05/30139247 DC | EN 14879-5. Organic coating systems and linings for protection of industrial apparatus and plants against corrosion caused by aggressive media. Part 5. Linings on concrete components | |
| 05/30139250 DC | EN 14879-4. Organic coating systems and linings for protection of industrial apparatus and plants against corrosion caused by aggressive media. Part 4. Linings on metallic components | |
| 05/30139335 DC | EN 12487. Corrosion protection of metals. Rinsed and non-rinsed chromate conversion coatings on aluminium and aluminium alloys | |
| 05/30139444 DC | ISO 7539-1. Corrosion of metals and alloys. Stress corrosion testing. Part 1. Guide to testing procedures | |
| 05/30139447 DC | ISO 21601. Guidelines for assessing the significance of stress corrosion cracks detected in service | |
| 05/30140324 DC | EN ISO 12944-5. Paints and varnishes. Corrosion protection of steel structures by protective paint systems. Part 5. Protective paint systems | |
| 05/30140928 DC | EN 15631. Determination of the influence of the corrosion protection on the anchorage capacity of the transverse anchorage bars | |
| 05/30140937 DC | ISO 10414-1. Petroleum and natural gas industries. Field testing of drilling fluids. Part 1. Water-based fluids | |
| 06/30145214 DC | EN 671-1. Fixed firefighting systems. Hose systems. Part 1. Hose reels with semi-rigid hose | |
| 06/30145217 DC | EN 671-2. Fixed firefighting systems. Hose systems. Part 2. Hose system with lay-flat hose | |
| 06/30146267 DC | ISO 11154. Road vehicles. Roof load carriers | |
| 06/30146724 DC | EN 10277-1. Bright steel products. Technical delivery conditions. Part 1. General | |
| 06/30149361 DC | ISO 13704. Petroleum, petrochemical and natural gas industries. Calculation of heater-tube thickness in petroleum refineries | |
| 06/30149450 DC | EN 1866-1. Mobile fire extinguishers. Part 1. Characteristics, performance and test methods | |
| 06/30149994 DC | EN ISO 12944-6. Paints and varnishes. Corrosion protection of steel structures by protective paint systems. Part 6. Laboratory performance test methods | |
| 06/30151472 DC | BS EN 4534-2. Aerospace series. Bushes, plain in aluminium alloy with self-lubricating liner, elevated load. Part 2. Dimensions and loads. Inch series | |
| 06/30151475 DC | BS EN 4535-2. Aerospace series. Bushes, flanged in aluminium alloy with self-lubricating liner, elevated load. Part 2. Dimensions and loads. Inch series | |
| 06/30151478 DC | BS EN 4536-2. Aerospace series. Bushes, plain in corrosion-resisting steel with selliner, elevated load. Part 2. Dimensions and loads. Inch series | |
| 06/30151481 DC | BS EN 4537-2. Aerospace series. Bushes, flanged in corrosion-resisting steel with sliner, elevated load. Part 2. Dimensions and loads. Inch series | |
| 06/30151546 DC | BS EN 4613. Aerospace series. Spherical plain bearings in corrosion resisting steel with self lubricating liner, narrow series. Dimensions and loads. Inch series | |
| 06/30151549 DC | BS EN 4614. Aerospace series. Spherical plain bearings in corrosion resisting steel with self lubricating liner, wide series. Dimensions and loads. Inch series | |
| 06/30152560 DC | BS IEC 60603-7. Connectors for electronic equipment. Part 7. Detail specification for 8-way, unshielded, free and fixed connectors | |
| 06/30155368 DC | EN 14879-6. Organic coating systems and linings for protection of industrial apparatus and plants against corrosion caused by aggressive media. Part 6. Combined linings with tile and brick layers | |
| 06/30155632 DC | EN 13260. Railway applications. Wheelsets and bogies. Wheelsets. Products requirements | |
| 06/30155635 DC | EN 13261. Railway applications. Wheelsets and bogies. Axles. Product requirements | |
| BS 5680:1979, ISO 5662-1978 | Method for detection of corrosive sulphur in petroleum-based electrical insulating oils | |
| BS 5903:1980 | Method for determination of resistance to intergranular corrosion of austenitic stainless steels: copper sulphate-sulphuric acid method (Moneypenny Strauss test) | |
| BS 6682:1986, ISO 7441-1984 | Method for the determination of bimetallic corrosion in outdoor exposure corrosion tests | |
| BS 1723-3:1988 | Brazing. Methods for non-destructive and destructive testing | |
| BS 6161-17:1990, ISO 8994:1989 | Methods of test for anodic oxidation coatings on aluminium and its alloys. Rating system for the evaluation of pitting corrosion. Grid method | |
| BS 6161-16:1990, ISO 8993:1989 | Methods of test for anodic oxidation coatings on aluminium and its alloys. Rating system for the evaluation of pitting corrosion. Chart method | |
| BS EN ISO 7539-7:1995 | Corrosion of metals and alloys. Stress corrosion testing. Slow strain rate testing | |
| BS 2000-112:1993 | Methods of test for petroleum and its products. Determination of corrosiveness to copper of lubricating grease. Copper strip method | |
| BS EN ISO 6251:1995, BS 2000:Part 411:1995, ISO 6251:1982 | Liquefied petroleum gases. Corrosiveness to copper. Copper strip test | |
| BS 7835:1996 | Specification for cables with extruded cross-linked polyethylene or ethylene propylene rubber insulation for rated voltages from 3800/6600 V up to 19 000/33 000 V having low emission of smoke and corrosive gases when affected by fire | |
| DD ENV 1965-2:1996 | Structural adhesives. Corrosion. Determination and classification of corrosion to a brass substrate | |
| BS 6917:1987, ISO 7384:1986 | Method for corrosion testing in artificial atmospheres: general principles | |
| BS 6918:1990, ISO 8044:1989 | Glossary of terms for corrosion of metals and alloys | |
| BS EN ISO 7539-6:1995 | Corrosion of metals and alloys. Stress corrosion testing. Preparation and use of pre-cracked specimens | |
| BS EN ISO 2160:1995, BS 2000:Part 154:1995, ISO 2160:1985 | Petroleum products. Corrosiveness to copper. Copper strip test | |
| BS EN 12472:1999 | Method for the simulation of wear and corrosion for the detection of nickel release from coated items | |
| BS 6580:1985 | Specification for corrosion inhibiting, engine coolant concentrate ('antifreeze') | |
| BS 6918:1987, ISO 8044-1986 | Glossary of terms for corrosion of metals and alloys | |
| BS 6924:1988, ISO 6251-1982 | Method for determination of corrosiveness of liquefied petroleum gases to copper | |
| BS 7479:1991, ISO 9227:1990 | Method for salt spray corrosion tests in artificial atmospheres | |
| BS 4959:1974 | Recommendations for corrosion and scale prevention in engine cooling water systems | |
| BS 5117:Part 0:1985 | Testing corrosion inhibiting, engine coolant concentrate ('antifreeze'). General introduction | |
| BS 2011-2.1Kc:1991 | Environmental testing. Tests. Test Kc and guidance. Sulphur dioxide test for contacts and connections | |
| BS 1391:1952 | Specification for performance tests for protective schemes used in the protection of light-gauge steel and wrought iron against corrosion | |
| BS 6121-3:1990 | Mechanical cable glands. Specification for special corrosion resistant glands | |
| BS 5117:Part 2:Section 2.3:1985 | Testing corrosion inhibiting, engine coolant concentrate ('antifreeze'). Methods of test for corrosion inhibition performance. Recirculating rig test | |
| DD 24:1973 | Recommendations for methods of protection against corrosion on light section steel used in building | |
| BS 6076:1981 | Specification for tubular polyethylene film for use as protective sleeving for buried iron pipes and fittings | |
| BS 3900:Part F12:1985, ISO 7253-1984 | Methods of test for paint. Durability tests on paint films. Determination of resistance to neutral salt spray | |
| BS EN ISO 4623:1995, BS 3900-F13:1986 | Paints and varnishes. Filiform corrosion test on steel | |
| BS 6724:1990 | Specification for armoured cables for electricity supply having thermosetting insulation with low emission of smoke and corrosive gases when affected by fire | |
| BS 7211:1994 | Specification for thermosetting insulated cables (non-armoured) for electric power and lighting with low emission of smoke and corrosive gases when affected by fire | |
| BS 903:Part A37:1979 | Physical testing of rubber. Assessment of adhesion to and corrosion of metals | |
| BS EN ISO 8403:1995 | Metallic coatings. Coatings anodic to the substrate. Rating of test specimens subjected to corrosion tests | |
| BS 6724:1986 | Specification for armoured cables for electricity supply having thermosetting insulation with low emission of smoke and corrosive gases when affected by fire | |
| BS 7211:1989 | Specification for thermosetting insulated cables (non-armoured) for electric power and lighting with low emission of smoke and corrosive gases when affected by fire | |
| BS 2000-112:2002 | Methods of test for petroleum and its products. Determination of corrosiveness to copper of lubricating grease. Copper strip method | |
| BS 2000:Part 154:1993 | Methods of test for petroleum and its products. Petroleum products. Corrosiveness to copper. Copper strip test | |
| BS 2000:Part 112:1982 | Methods of test for petroleum and its products. Corrosive substances in grease (copper strip test) | |
| BS AU 148-10:1969 | Methods of test for motor vehicle paints. Resistance to heat and corrosion | |
| PD 6583:1993, ISO TR 10271:1993 | Dentistry. Information on methods available for the determination of tarnish and corrosion of metals and alloys | |
| DD ENV 1965-1:1996 | Structural adhesives. Corrosion. Determination and classification of corrosion to a copper substrate | |
| BS EN 1303:1998 | Building hardware. Cylinders for locks. Requirements and test methods | |
| BS EN ISO 1462:1995 | Metallic coatings. Coatings other than those anodic to the basis metal. Accelerated corrosion tests. Method for the evaluation of results | |
| BS EN 3-5:1996 | Portable fire extinguishers. Specification and supplementary tests | |
| PD 6466:1976 | Sulphur dioxide (SO) corrosion test cabinet | |
| BS 5593:1978 | Specification for impregnated paper-insulated cables with aluminium sheath/neutral conductor and three shaped solid aluminium phase conductors (CONSAC), 600/1000 V, for electricity supply | |
| BS 6161-4:1981, ISO 2932:1981 | Methods of test for anodic oxidation coatings on aluminium and its alloys. Assessment of sealing quality by measurement of the loss of mass after immersion in acid solution | |
| BS 3313-2:1968 | Specification for aluminium capping foil and strip for dairy product containers. Aluminium capping foil for skirted closures for plastics containers | |
| BS 4487:1969 | Specification for inhibited 1,1,1-trichloroethane (methylchloroform) | |
| BS 2000:Part 154:1982 | Methods of test for petroleum and its products. Detection of copper corrosion from petroleum products by the copper strip tarnish test | |
| BS 3761:1970 | Specification for non-flammable solvent-based paint remover | |
| BS 5117:1974 | Methods of test for corrosion inhibition performance of antifreeze solutions | |
| BS 2011-2.1Ka:1982, IEC 60068-2-11:1981 | Environmental testing. Tests. Test Ka.Salt mist | |
| BS 2516:1954 | Specification for tail lights for vehicles, including cycles | |
| BS 3107:1973 | Specification for small incinerators | |
| BS 5720:1979 | Code of practice for mechanical ventilation and air conditioning in buildings | |
| BS 1619-1:1962 | Re-usable hypodermic syringes for insulin injection. Specification for syringes for use with insulin of strengths 20, 40 and 80 units per millilitre | |
| BS AU 148-11:1969 | Methods of test for motor vehicle paints. Resistance to blistering | |
| BS AU 148-13:1969 | Methods of test for motor vehicle paints. Resistance to deterioration by contact with other materials | |
| BS AU 148-14:1969 | Methods of test for motor vehicle paints. Resistance to outdoor exposure | |
| BS AU 183:1983 | Specification for passive seat belt systems | |
| BS AU 186a:1983 | Specification for carry cot restraints | |
| BS 2455:Part 1:1973 | Sampling and examining deposits from boilers and associated industrial plant. Water-side deposits | |
| BS 2455:Part 2:1983 | Sampling and examining deposits from boilers and associated industrial plant. Methods for sampling and examining fire-side deposits | |
| BS 4839-1:1972 | Plastics containers. Containers up to 5 litres capacity | |
| BS 4839-2:1974 | Plastics containers. Containers over 5 litres and up to 60 litres capacity | |
| BS S 528:1970 | Specification for 23/14 chromium-nickel heat-resisting steel sheet and strip (titanium stabilized: 54 hbar) (elevated temperature properties not verified) | |
| BS S 529:1970 | Specification for 23/14 chromium-nickel heat-resisting steel sheet and strip (niobium stabilized: 54 hbar) (elevated temperature properties not verified) | |
| BS S 531:1970 | Specification for 24/17 chromium-nickel heat-resisting steel sheet and strip (niobium stabilized: 54 hbar) (elevated temperature properties not verified) | |
| BS 8010-2.4:1988 | Code of practice for pipelines. Pipelines on land: design, construction and installation. Prestressed concreted pressure pipelines | |
| BS 3254-1:1988 | Seat belt assemblies for road vehicles. Specification for restraining devices for adults | |
| BS 8010-2.3:1988 | Code of practice for pipelines. Pipelines on land: design, construction and installation. Asbestos cement | |
| BS 1133-6.2:1991 | Packaging code. Protection of metal surfaces against corrosion during transport and storage. Temporary protectives and their application | |
| BS 1683:1967 | Specification for coated aluminium foil for wrapping processed cheese | |
| BS 1133-6.1:1991 | Packaging code. Protection of metal surfaces against corrosion during transport and storage. Cleaning and drying of metal surfaces | |
| BS 7541:1992 | Specification for temporary protectives for the protection of metal surfaces against corrosion during transport and storage | |
| BS 7673:1993 | Specification for domestic gas cooker oven control valves with or without manual override | |
| BS EN 60249-1:1993, IEC 60249-1:1982 | Base materials for printed circuits. Base materials for printed circuits. Test methods | |
| BS 3254-2:1991 | Seat belt assemblies for road vehicles. Specification for restraining devices for children | |
| BS AU 202b:1995 | Specification for rearward-facing restraint systems for infants, for use in road vehicles | |
| BS EN 60249-2-19:1993, IEC 60249-2-19:1992 | Specifications. Specification No. 19. Thin bismaleimide/triazine modified epoxide woven glass fabric copper-clad laminated sheet of defined flammability for use in the fabrication of multilayer printed boards | |
| BS 611:Part 1:1978 | Petri dishes. Specification for glass Petri dishes | |
| BS 1348:1970 | Specification for kitchen measuring spoons, measures and jugs | |
| BS 2579:1955 | Specification for solid drawn copper alloy tubes for the manufacture of screwed ferrules, and copper alloy screwed ferrules for condenser, evaporator, heater and cooler tubes | |
| BS 2983:1958 | Specification for hypodermic dental needles | |
| BS 3456:Part A:Section A1:1966 | Specification for safety of household and similar electrical appliances. Heating and cooking appliances. General requirements | |
| BS 3634:1963 | Specification for black bitumen oil varnish | |
| BS EN 60691:1996 | Thermal links. Requirements and application guide | |
| BS EN ISO 4540:1995 | Metallic coatings. Coatings cathodic to the substrate. Rating of electroplated test specimens subjected to corrosion tests | |
| BS 953:1979 | Methods of test for safety and protective footwear | |
| BS EN 10155:1993 | Structural steels with improved atmospheric corrosion resistance. Technical delivery conditions | |
| BS 709:1983 | Methods of destructive testing fusion welded joints and weld metal in steel | |
| BS 1840:1960 | Specification for steel columns for street lighting | |
| BS 2515:1954 | Specification for reflex reflectors for vehicles, including cycles | |
| BS 2486:1978 | Recommendations for treatment of water for land boilers | |
| BS EN 60695-5-1:1993 | Fire hazard testing. Assessment of potential corrosion damage by fire effluent. General guidance | |
| BS 2011:Part 2.1Kc:1977 | Environmental testing. Tests. Test Kc. Sulphur dioxide test for contacts and connections | |
| BS 3130:Part 1:1973 | Glossary of packaging terms. General | |
| BS 4292:1968 | Specification for electroplated coatings of gold and gold alloy | |
| BS 1224:1970 | Specification for electroplated coatings of nickel and chromium | |
| BS 3657:1963 | Specification for blue-black writing inks | |
| BS 3740:1964 | Specification for steel plate clad with corrosion-resisting steel | |
| BS 5124:1975 | Specification for plastic crates to hold 20 one pint milk bottles | |
| BS 5362:1976 | Specification for rolling bearing greases | |
| BS 5365:Part 1:1976, ISO 3137-1974 | Methods of sampling and test for anhydrous hydrogen fluoride for industrial use. Sampling | |
| BS 5365:Part 2:1976, ISO 3138-1974 | Methods of sampling and test for anhydrous hydrogen fluoride for industrial use. Determination of non-volatile acid content: titrimetric method | |
| BS 5365:Part 5:1979, ISO 3702-1976 | Methods of sampling and test for anhydrous hydrogen fluoride for industrial use. Determination of sulphur dioxide content | |
| DD ENV 13797:2001 | Corrosion protection. Carbon and low alloy steels for use in hydrogen sulfide containing environments in oil and gas production. Materials and test methods. Guidelines | |
| BS 2011-2.1Kd:1977, IEC 60068-2-43:1976 | Environmental testing. Tests. Test Kd. Hydrogen sulphide test for contacts and connections | |
| BS 5466:Part 1:1977, ISO 3768-1976 | Methods for corrosion testing of metallic coatings. Neutral salt spray test (NSS test) | |
| BS EN 990:1996 | Test methods for verification of corrosion protection of reinforcement in autoclaved aerated concrete and lightweight aggregate concrete with open structure | |
| BS EN 60512-11-7:1997, IEC 60512-11-7:1996 | Connectors for electronic equipment. Tests and measurements. Climatic tests. Test 11g. Flowing mixed gas corrosion test | |
| BS 534:1981 | Specification for steel pipes and specials for water and sewage | |
| BS 1615:1972 | Specification for anodic oxidation coatings on aluminium | |
| BS 7352:1990 | Specification for strength and durability performance of metal hinges for side hanging applications and dimensional requirements for template drilled hinges | |
| BS ISO 13806:1999 | Vitreous and porcelain enamels. Corrosion tests in closed systems | |
| BS 3100:1976 | Specification for steel castings for general engineering purposes | |
| BS 2569:Part 1:1964 | Specification for sprayed metal coatings. Protection of iron and steel by aluminium and zinc against atmospheric corrosion | |
| BS 5466:Part 3:1977, ISO 3770-1976 | Methods for corrosion testing of metallic coatings. Copper-accelerated acetic acid salt spray test (CASS test) | |
| BS 148:1972 | Specification for insulating oil for transformers and switchgear | |
| BS 5466:Part 2:1977, ISO 3769-1976 | Methods for corrosion testing of metallic coatings. Acetic acid salt spray test (ASS test) | |
| CP 2010:Part 3:1972 | Pipelines. Design and construction of iron pipelines in land | |
| BS 4110:1979 | Specification for eye-protectors for vehicle users | |
| BS 903:Part A37:1987 | Physical testing of rubber. Determination of adhesion to and corrosion of metals | |
| BS 7846:1996 | Specification for 600/1000 V armoured fire-resistant electric cables having low emission of smoke and corrosive gases when affected by fire | |
| BS EN 60512-11-14:1997, IEC 60512-11-14:1996 | Connectors for electronic equipment. Tests and measurements. Climatic tests. Test 11p. Flowing single gas corrosion test | |
| BS 1133:Section 6:1966 | Packaging code. Temporary protection of metal surfaces against corrosion (during transport and storage) | |
| BS 1504:1976 | Specification for steel castings for pressure purposes | |
| BS 5977-2:1983 | Lintels. Specification for prefabricated lintels | |
| BS 5365:Part 3:1979, ISO 3699-1976 | Methods of sampling and test for anhydrous hydrogen fluoride for industrial use. Determination of water content (Karl Fischer method) | |
| BS 3900:Part G5:1976 | Methods of test for paints. Environmental tests on paint films (including tests for resistance to corrosion and chemicals). Determination of resistance to liquids | |
| BS 5365:Part 6:1981, ISO 3700-1980 | Methods of sampling and test for anhydrous hydrogen fluoride for industrial use. Determination of water content (conductimetric method) | |
| BS 6469-5.1:1992, IEC 60811-5-1:1990 | Insulating and sheathing materials of electric cables. Methods of test specific to filling compounds. Drop-point. Separation of oil. Lower temperature brittleness. Total acid number. Absence of corrosive components. Permittivity at 23°C. D.C. resistivity at 23°C and 100°C | |
| BS 3900-F18:1998, ISO 11997-1:1998 | Methods of test for paint. Durability tests on paint films. Determination of resistance to corrosion under a wet (salt fog)/dry/humidity cycle | |
| BS AU 148-2:1969 | Methods of test for motor vehicle paints. Resistance to continuous salt spray | |
| BS 7655-8.2:1997 | Specification for insulating and sheathing materials for cables. Cross-linked sheathing compounds having low emission of corrosive gases, and suitable for use in cables having low emission of smoke when affected by fire. Ordinary duty oil-resisting types | |
| BS 3581:1963 | Specification for stainless steel cone joint pipe fittings | |
| BS 5365:Part 4:1979, ISO 3701-1976 | Methods of sampling and test for anhydrous hydrogen fluoride for industrial use. Determination of hexafluorosilicic acid content | |
| BS 5366:1976, ISO 3139-1976 | Methods of sampling and test for aqueous hydrofluoric acid for industrial use | |
| BS 1501:Part 3:1973 | Specification for steels for fired and unfired pressure vessels. Plates. Corrosion and heat resisting steels. Imperial units | |
| BS 6136:1981 | Specification for dental tweezers | |
| CP 1014:1963 | Protection of electrical power equipment against climatic conditions | |
| BS AU 40:Part 6:1968 | Specification for motor vehicle lighting and signalling equipment. Headlamps for mechanically assisted pedal cycles (mopeds) | |
| BS AU 157b:1982 | Specification for children's restraining devices | |
| BS AU 160c:1971 | Specification for seat belt assemblies for motor vehicles | |
| BS X 28:1966 | Specification for matt synthetic finishing scheme for aeronautical purposes | |
| BS EN 60249-2-4:1994, IEC 60249-2-4:1987 | Specifications. Specification for epoxide woven glass fabric copper-clad laminated sheet, general purpose grade. Specification No. 4: Epoxide woven glass fabric copper-clad laminated sheet, general purpose grade | |
| BS EN 60249-2-3:1994, IEC 60249-2-3:1987 | Specifications. Metal-clad base materials for printed wiring boards. Copper-clad base material. Specification for epoxide cellulose paper copper-clad laminated sheet of defined flammability (vertical burning test). Specification No. 3: Epoxide cellulose paper copper-clad laminated sheet of defined flammability (vertical burning test) | |
| BS EN 60249-2-9:1994, IEC 60249-2-9:1987 | Specifications. Epoxide cellulose paper core, epoxide glass cloth surfaces copper-clad laminated sheet of defined flammability (vertical burning test). Specification No.9:Epoxide cellulose paper core, epoxide glass cloth surfaces copper-clad laminated sheet of defined flammability (vertical burning test) | |
| BS EN 60249-2-17:1993, IEC 60249-2-17:1992 | Specifications. Specification No. 17. Thin polyimide woven glass fabric copper-clad laminated sheet of defined flammability for use in the fabrication of multilayer printed boards. Specification No.17: Thin polyimide woven glass fabric copper-clad laminated sheet of defined flammability for use in the fabrication of multilayer printed boards | |
| BS EN 60249-2-18:1993, IEC 60249-2-18:1992 | Specifications. Specification No. 18. Bismaleimide/triazine modified epoxide woven glass fabric copper-clad laminated sheet of defined flammability (vertical burning test). Specification No.18: Bismaleimide/triazine modified epoxide woven glass fabric copper-clad laminated sheet of defined flammability (vertical burning test) | |
| BS ISO 1458:2002 | Metallic coatings. Electrodeposited coatings of nickel | |
| BS 3680-9A:1971 | Methods of measurement of liquid flow in open channels. Water level instruments. Specification for the installation and performance of pressure actuated liquid level measuring equipment | |
| BS 6425-2:1993 | Test on gases evolved during the combustion of materials from cables. Determination of degree of acidity (corrosivity) of gases by measuring pH and conductivity | |
| BS 1400:1973 | Specification for copper alloy ingots and copper and copper alloy castings | |