Retail Price: N.A. Now Selling at: US$200 Hardcover, 382 pages CONVERSION COATINGSA Reference for Phosphating, Chromating, and Anodizing ProcessesC Rajagopal & K I Vasu
Table of Contents |
|
|
PART ONE Phosphate Coatings |
||
1. Introduction |
3 | |
2. Historical Background |
5 | |
3. Principles of Corrosion |
8 | |
4. Surface Preparation and Pre-treatment Processes |
23 | |
5. Theoretical Aspects of Phosphating |
40 | |
6. Types of Phosphate Coatings |
50 | |
7. Methods of Phosphating |
56 | |
8. Properties of Phosphate Coatings and Influencing Factors |
62 | |
9. Practical Applications and Uses of Phosphating: With and without Post-treatments |
71 | |
10. Phosphate Coatings on Non-ferrous Metals and Other Specialized Processes |
85 | |
11. Some Recent Innovations in Phosphating |
100 | |
12. Analytical and Quality Controls |
105 | |
13. Evaluation and Testing of Phosphate Coatings |
118 | |
14. Assessment of Phosphate Coatings |
136 | |
15. Plant Requirements |
148 | |
16. Solution Maintenance Schedules |
155 | |
17. Pollution Control, Effluent Treatment and Waste Disposal |
159 | |
18. Safety Precautions |
169 | |
19. National and International Standards on Phosphating |
172 | |
PART Two Oxide and Chromate Coatings |
||
20. Oxide and Chromate Conversion Coatings |
179 | |
21. Chromate Treatment of Metals |
185 | |
22. General Properties of Chromate Films and Their Uses |
189 | |
23. Chromate Treatment for Zinc and Cadmium |
197 | |
24. Chromate Treatments for Copper and its Alloys |
205 | |
25. Chromate Treatments for Aluminium |
207 | |
26. Film Formation and Factors Influencing Mechanism |
212 | |
27. Methods of Applying Chromate Coatings |
219 | |
28. Evaluation of Chromate Coatings |
222 | |
29. Troubleshooting |
233 | |
30. Pollution Control |
240 | |
31. Specifications for Testing Chromate Conversion Coatings |
243 | |
PART THREE Anodizing |
||
32 Anodizing of Aluminium and Its Alloys |
247 | |
33. Pre-treatment Processes of Aluminium and Its Alloys for Anodizing |
261 | |
34. Colouring of Anodized Aluminium |
286 | |
35. Anodizing Plant Equipment and Accessories |
295 | |
36. Sealing of Anodic Oxide Coatings |
311 | |
37. Quality Control and Testing of Anodic Oxide Films |
318 | |
38. Control and Maintenance of Anodizing Bath |
343 | |
39. Effluent Treatment and Recovery of Chemicals in Anodizing Processes |
356 | |
References |
360 | |
Index |
375 | |
|
Publisher: Tata McGraw-Hill Publishing Company Limited |
||